Because the film is only microns thick, the pitch diameter of an M2 thread is effectively unchanged and the part can be supplied to the original thread tolerance. Wear resistance comes from hardness — nitride films commonly exceed 1500 HV — but impact resistance is lower than a plated layer, so the driver bit should not be allowed to chatter against the head.
installed by electric driver, avoiding tip contact with the film.
Use a bit with controlled magnetic force to avoid scratching the film and exposing the substrate.
| Drive Type | Torx T |
|---|---|
| Head Type | Ultra Low Profile / CD-textured |
| Surface Treatment | PVD Vacuum Coating (CD-textured / colored) |
| Standard | GB/T 3098.1, GB/T 9791 (coating verification) |
| Drive | star recess |
| Installation | electric driver, avoiding tip contact with the film |
| Typical substrate | visible parts and wearables |
| Key inspections | film thickness, colour, adhesion |
Colour is checked against a master plaque with a spectrophotometer, with ΔE held inside the agreed window.Alternative materials and finishes can be quoted side by side during sampling, so cost and corrosion resistance can be traded off explicitly.